- FAULTS:
A. Because of intensive wear of the guides resulting from friction with the ballast, in a few years of use of the equipment, partial or complete wear is seen,
resulting in plough deformation, cracks and decrease in overall strength of the structure.
B. Deformation of the ploughs resulting from bumps (dead sleepers, pieces of rail in the ballast, etc) leading in turn to their deformation and disturbances in the normal functioning of the ballast distributing machine.
-REPAIR WORK :
A. Using a technique developed by the company, full recovery is done through semi-automatic surface welding of the lower guides (with high strength manganese wire – up to three layers); fastening of the guides to the ploughs and removal of cracks in the connecting seams between the ploughs and the supporting strut.
B. Alignment of deformed ploughs, monitoring check of the geometrical dimensions and the admissible horizontal deviation of the lower guides.
- OTHER TECHNOLOGICAL REPAIR OPTIONS:
In the case of external and internal wear of the ploughs (decreased wall thickness) resulting from friction with the ballast, the company offers removal of the ploughs or several protection options for them through tin coating (ordinary steel sheets, manganese wear-resistant tin or tin with a surface-welded wear resistant layer) or simple protection through metal cladding. The manufacture of new ploughs and other parts from manganese highly resistant steel.
|